Customization: | Available |
---|---|
Application: | Metallurgical Industry |
Carbon Content: | High-Carbon |
Suppliers with verified business licenses
Property | KBD-5 | KBD-6 | KBD-7 | KBD-7B | KBD-8 | Unit |
Apparent Density | 1.85 | 1.90 | 1.82 | 1.82 | 1.90 | g/cm3 |
Max Grain Size | 13-15 | 8-10 | 8-10 | 13-15 | 8-10 | µm |
Ash value | ≤500 | ≤500 | ≤500 | ≤500 | ≤500 | ppm |
Specific Electrical Resistivity | 8-10 | 8-9 | 11-13 | 11-13 | 11-13 | μΩm |
Flexural Strength | 46 | 55 | 51 | 59 | 60 | Mpa |
Compressive Strength | 85 | 95 | 115 | 121 | 135 | Mpa |
Shore Hardness | 48 | 53 | 65 | 70 | 70 | HSD |
Thermal Expansion (room temperature to 600ºC) | 4.75 | 4.8 | 5.8 | 5.8 | 5.85 | 10-6/ºC |
Property | KBG-4 | KBG-5 | Unit |
Apparent Density | ≥1.80 | ≥1.85 | g/cm3 |
Ash value | ≤500 | ≤500 | ppm |
Shore Hardness | ≥40 | ≥45 | HSD |
Specific Electrical Resistivity | ≤12 | ≤12 | μΩm |
Flexural Strength | 38 | 41 | Mpa |
Compressive Strength | 81 | 87 | Mpa |
Max Grain Size | 25 | 25 | μm |
Property | TSK | GSK | Unit |
Apparent Density | ≥1.70 | ≥1.72 | g/cm3 |
Max Grain Size | ≤2 | ≤0.8 | mm |
Specific Electrical Resistivity | 8-10 | ≤8.5 | μΩm |
Flexural Strength | ≥12.5 | ≥15 | Mpa |
Compressive Strength | ≥28 | ≥35 | Mpa |
Porosity | ≤24 | ≤20 | % |
Ash value | ≤0.3 | ≤0.3 | % |